1.840-inch NPS Sendust Magnetic Powder Core with Nice Temperature Stability, Made of FeSiAlNew
1.840-inch NPS Sendust Magnetic Powder Core with Nice Temperature Stability, Made of FeSiAlNew
1.840-inch NPS Sendust Magnetic Powder Core with Nice Temperature Stability, Made of FeSiAlNew
1.840-inch NPS Sendust Magnetic Powder Core with Nice Temperature Stability, Made of FeSiAlNew

1 / 2

1.840-inch NPS Sendust Magnetic Powder Core with Nice Temperature Stability, Made of FeSiAlNew

Get Latest Price
Send Inquiry
Model No. : Shirui-NPS184125-1-1-1-1
Brand Name :

Product description

  • Material: FeSiAl
  • Characteristics:
    • PPF series core: 6.5% silicon iron distributed gapped powder core
    • Nice temperature stability
    • Lower loss than powder iron magnetic cores
    • Significantly lower loss than powder iron cores
    • Excellent DC bias performance
    • High saturation flux density
    • Binding with inorganic only
    • Neither aging nor instability issue
    • No noise
    • Lower cost than MPP core
    • Customized requirements and appearance or characteristics are accepted
    • High-efficiency
    • High PPR (performance to price ratio)
  • Advantages:
    • Wide range permeability: 26 to 90μ
    • Lower core loss better DC bias
  • Specifications:
    • AL: 281nH/N2
    • Permeability: 125μ
    • Bare core:
      • Outer diameter: 46.74mm/1.840-inch
      • Inner diameter: 24.13mm/0.950-inch
      • HT: 18.03mm/0.710-inch
    • Coated core:
      • Outer diameter: 47.63mm/1.875-inch
      • Inner diameter: 23.32mm/0.918-inch
      • HT: 18.92mm/0.745-inch
    • Core loss: medium
    • DC bias: nice
    • Curie temperature: 600°C
    • Flux density: 10,000g/cm³
    • Outer diameter: 0.140 to 3.063-inch
    • Permeability: 26 to 173μ
    • Shapes: E, U, block and toroidal
  • Applications:
    • PFC chokes for large current
    • Reactor for electric vehicles/air condition
    • Power inductor for fuel cell vehicles
    • In line noise filters
    • EMI filters
    • Boost inductors
    • Switching regulator inductors
  • PPF series core: 6.5% silicon iron distributed gapped powder core
  • Nice temperature stability
  • Lower loss than powder iron magnetic cores
  • Significantly lower loss than powder iron cores
  • Excellent DC bias performance
  • High saturation flux density
  • Binding with inorganic only
  • Neither aging nor instability issue
  • No noise
  • Lower cost than MPP core
  • Customized requirements and appearance or characteristics are accepted
  • High-efficiency
  • High PPR (performance to price ratio)
  • Wide range permeability: 26 to 90μ
  • Lower core loss better DC bias
  • AL: 281nH/N2
  • Permeability: 125μ
  • Bare core:
    • Outer diameter: 46.74mm/1.840-inch
    • Inner diameter: 24.13mm/0.950-inch
    • HT: 18.03mm/0.710-inch
  • Coated core:
    • Outer diameter: 47.63mm/1.875-inch
    • Inner diameter: 23.32mm/0.918-inch
    • HT: 18.92mm/0.745-inch
  • Core loss: medium
  • DC bias: nice
  • Curie temperature: 600°C
  • Flux density: 10,000g/cm³
  • Outer diameter: 0.140 to 3.063-inch
  • Permeability: 26 to 173μ
  • Shapes: E, U, block and toroidal
  • Outer diameter: 46.74mm/1.840-inch
  • Inner diameter: 24.13mm/0.950-inch
  • HT: 18.03mm/0.710-inch
  • Outer diameter: 47.63mm/1.875-inch
  • Inner diameter: 23.32mm/0.918-inch
  • HT: 18.92mm/0.745-inch
  • PFC chokes for large current
  • Reactor for electric vehicles/air condition
  • Power inductor for fuel cell vehicles
  • In line noise filters
  • EMI filters
  • Boost inductors
  • Switching regulator inductors
  • Send Inquiry

    Product Alert

    Subscribe to your interested keywords. We will send freely the latest and hottest products to your Inbox. Don't miss any trade information.

    版权所有 © 宁波全贸信息技术有限公司 浙ICP备12012821号-1 浙B2-20200628