Manganese Aluminum Tablet Titanium Additive Model: 75Ti/80Ti Copper Additive Model: 75Cu/80C
Manganese Additive Model: 75Mn/80Mn/85Mn Iron Additive Model:75Fe/80Fe
Chromium Additive Model: 75Cr/80Cr Aluminum Strontium Alloy Model: AL-Sr10
Usage After finish alloying, Keep the temperature at 730-745°C and then put the aluminum strontium alloy in it for 10 mins, mix and refine fully for another 10 mins with high-purity nitrogen or argon gas, finallly anneal for 25 Minutes is ok. Benefits of Intermediate Alloy · Rapid dissolution at normal casthouse operating temperatures. · Concentrated form–means reduced inventory, transport and storage costs compared with binary master alloys. · High element recovery · Minimal temperature loss upon addition. · Clean and accurate addition. · Rapid, consistent solubility of self-sinking briquettes means less energy and less cost. · Color-as pictures Package and Conserve
2KG/Bag, 40KG/Box, 1000KG/Dozen, keep in ventilated and dry environment. Guarantee period 12 Month. Packages deposeed together and Don't put into stove to burn .