3TREES Low VOC Healthy Nail Adhesive Construction Adhesive
| ||
Discription:It is applicable to panel manufacturing, furniture manufacture and decorations. It can be widely used in bonding of fire-proof boards, aluminium-plastic panel, plywood, raw wooden boards, floors, bamboo materials, plastic boards, foam tape, wall paper, carpets, leather, rubber, metal materials, ceramic and textile materials etc.
| |||
Packing size: | 0.5KG, 1.7KG, 2KG, 2.3KG, | ||
Adhesion range: | 2300-3500MPa.s(23±2℃) | ||
Touch dry: | 10-25min. (23±2℃ with the humidity ≤75%) | ||
Thorough dry: | ≥36h | ||
Features: | 1.Odourless | ||
2.Ultra strong adhesion | |||
3.Good thermol resistance | |||
4.Anti-aging and durable | |||
5.Easy application | |||
Construction process: | 1.Make sure the surface of the adhesive material is clean and dry, keep the adhesive surface free of dust, grease. Roughening the surface if needed. | ||
2.A thin layer of the adhesive to be applied on both surfaces byscraper or roller. | |||
3.Leave for 10-25 minutes untill surface dry for better adhesion (surface drying time may vary according to the differences of temperature and humidity). | |||
4.Ensure the full contact of the both surface by adding pressure or hammering. |
Problem | Causes | Solutions |
Sticky Adhesive Membrane | 1. The temperature is too low, slow solvent evaporation or thick membrane. 2. Open time is not enough, bonding too early.
| 1 Immerse the all-purpose adhesive in 30°C-50°C water for 15- 25 minutes, then brush. 2 Prolonged open time, according to the temperature and humidity conditions to select the best adhesion time
|
Loose Adhesive Layer | Drying time too short, glue contains solvent Too thick membrane Adhesive layer contains air particles Too high humidity Too much moisture on applied surface Lack of applied pressure | Increase drying time appropriately Even applying, thin layer more times Apply at drying environment Dry the surface before applying Apply even pressure after application. |
Adhesive Membrane Cracking | Applied surfaces not matching Lack of enough adhesive Too much pressure applied, adhesive been squeezed out Low viscosity | Trial should be done before apply Apply evenly Apply adequate pressure
|
Weak Bonding Strength | Dirty surface Rough surface Too long or short drying time Humid environment low temperature Over-adhesive force Uncleaned surface before re-coating | Clean the surface Re-structure the surface Control drying time Apply supplementary heating methods Clean away the old membrane Reduce solvent amount |
Rough Adhesive Membrane | High humidity Using expired adhesive | Make sure ventilation Use guaranteed adhesive |
After application: Edge peeling, Corner peeling, Bubbling | Uneven adhesive application High humidity Too short drying time 4.Lack of enough adhesive 5.Surface deformation | 1. Even apply 2. Ventilation or apply supplementary heating methods 3. Control drying time 4. Even applying, thin layer more times 5. Use better quality surfaces
|