Product description
Major grade of cermet: MC102, MC911, MC206, MC509
Performance parameters of MC102:
- Density: 6.95g/cm3
- Hardness HRA: 92.5
- Flexural strength: 1,800N/mm2
- Fracture toughness: 10.5
- Features: on the premise of ensuring strength, it has high red-hardness and wear resistance, suitable for the finishing and ultra-fine finishing in low load and low impact force condition to the processing of bearing steel, carbon steel, low alloy steel and gray cast iron
- Usage: finish turning
- Equivalent to classification of ISO: P01-P05 and K01-K05
Performance parameters of MC206:
- Density: 7.0g/cm3
- Hardness HRA: 92.5
- Flexural strength: 2,300N/mm2
- Fracture toughness: 11.2
- Features: high strength, high wear resistance and low friction coefficient, suitable for finishing and semi-finishing of mild steel, normalizing gear steel, gray cast iron and ductile iron
- Usages: turning and milling
- Equivalent to classification of ISO: K05-K10, P01-P10 and M05-M10
Performance parameters of MC509:
- Density: 7.1g/cm3
- Hardness HRA: 92.1
- Flexural strength: 2,800N/mm2
- Fracture toughness: 12.4
- Features: high toughness and may bear heavy impact load
- General used for milling, medium-rough turning of soft steel, gray cast iron, Al alloy and bearing steel
- Usages: milling and wearing piece
- Equivalent to classification of ISO: P10-P20 and K10-K20
Performance parameters of MC911:
- Density: 7.05g/cm3
- Hardness HRA: 92.3
- Flexural strength: 2,000N/mm2
- Fracture toughness: 11.3
Performance between MC102 and MC509:
- It is hard to form crescent depression and suffered some impact, high heat-resistance
- Suitable for semi-finishing of soft steel, gray cast iron, Al alloy and bearing steel, and finishing of stainless
- Usages: turning and milling
- Equivalent to classification of ISO: P05-P15, K05-K15 and M05-M20
Density: 6.95g/cm3
Hardness HRA: 92.5
Flexural strength: 1,800N/mm2
Fracture toughness: 10.5
Features: on the premise of ensuring strength, it has high red-hardness and wear resistance, suitable for the finishing and ultra-fine finishing in low load and low impact force condition to the processing of bearing steel, carbon steel, low alloy steel and gray cast iron
Usage: finish turning
Equivalent to classification of ISO: P01-P05 and K01-K05
Density: 7.0g/cm3
Hardness HRA: 92.5
Flexural strength: 2,300N/mm2
Fracture toughness: 11.2
Features: high strength, high wear resistance and low friction coefficient, suitable for finishing and semi-finishing of mild steel, normalizing gear steel, gray cast iron and ductile iron
Usages: turning and milling
Equivalent to classification of ISO: K05-K10, P01-P10 and M05-M10
Density: 7.1g/cm3
Hardness HRA: 92.1
Flexural strength: 2,800N/mm2
Fracture toughness: 12.4
Features: high toughness and may bear heavy impact load
General used for milling, medium-rough turning of soft steel, gray cast iron, Al alloy and bearing steel
Usages: milling and wearing piece
Equivalent to classification of ISO: P10-P20 and K10-K20
Density: 7.05g/cm3
Hardness HRA: 92.3
Flexural strength: 2,000N/mm2
Fracture toughness: 11.3
It is hard to form crescent depression and suffered some impact, high heat-resistance
Suitable for semi-finishing of soft steel, gray cast iron, Al alloy and bearing steel, and finishing of stainless
Usages: turning and milling
Equivalent to classification of ISO: P05-P15, K05-K15 and M05-M20