Product description
FC filling mixture for ladle Manufacture : 1.Use the excellent Chrome Mineral sand and silicate sand as main raw material ; 2.Add the bonding agent ; 3.Mix them even according to the grain size distrbution . Products feature. 1.low sinter temperature (1200 °C) 2.Slim liquid facing steel water; 3.Effective flowing speed ; 4.High opening rate 98% Application: Used for ladle . Index:
Item | Cr2O3(%) | SiO2 (%) | MgO (%) |
Chrome GB-1 | 20-26 | 22-26 | - |