Reinforced composite Material | Din52913 Stabillty Compressive stress(N/mm2) | Temperature | ASRMF36A -66 Compressibility% | ASEMF36A-66 Recovery% | Dn3535 Gas permeability(cm2/min) |
In oxidzing Media | In nonoxidizing Media |
Tanged Carbon steel Sheet (Tickness 0.20-0.25mm) | ≥ 48 | -10-450 | -10-550 | 30-35 | 15-20 | ≤ 0.8 |
Ss304,316Tanged stainless steel Sheet (Tickness 0.1mm) | ≥ 48 | -240-450 | -200-560 (Ss304) -200-870 (Ss316) | 30-40 | 15-30 | ≤ 0.8 |
Ss304 ,316 Stainless steel flat sheet (Tickness 0.1mm) | ≥ 45 | -240-450 | -200-560 (Ss304) -220-870 (Ss316) | 40-50 | 10-15 | ≤ 0.4 |
Ss304 ,316 stainless steel mesh | ≥ 40 | -240-450 | -200-560 (Ss304) -220-870 (Ss316) | 30-35 | 15-20 | ≤ 1.0 |
Mylar reinforced (Tickness 0.05mm) | ≥ 40 | -240-450 | -200-1650 | 40-50 | 10-15 | ≤ 0.4 |