Features of pad printing silicon rubber


1. be exquisite

2. without granules or impurity

3. has advantages of wearability and resilience.


Applications of pad printing silicon rubber


Pad printing silicon rubber is specially designed for making printing pads . It is mainly used for printing irregular patterns of plastic toys, electroplating products, electronic toys, trademarks, etc.


Operation instruction for pad printing silicon


1.Washand clean molds with detergents, dry the molds and use an air gun if necessary, and apply a film of mold release.


2. Determine the normal proportion of pad printing silicon and silicon oil on the basis of customer requirements. Add more silicon oils if a larger area of printed pattern and therefore soft rubber head is needed by the customer. Otherwise, add no or less silicon oil for better hardness. For normal pad printing rubber head, hardness between15 A°--25A°will be appropriate. If excessive amount of silicon oil is added, the number of printing will be limited by an extremely soft rubber head, and the molecular weight of silicon of however supreme quality will be destroyed by silicon oil, and therefore, the phenomenon of compromised resistance to abrasion, solvent and aging.


3. The normal proportion is as follows:100gsilicon admixed with30gsilicon oil for a hardness of20 A° will be suitable for pad printing for alloy toy cars and products with small patterns and contact area. If larger pressure contact surface or soft rubber head is required, the silicon and silicon oil proportion can be adjusted to 100:50, 100:80 and so on. Remember, the more silicon oil is added, the softer the rubber head will be, and the number of pad printing, resistance to abrasion and solvent will be undermined, and hence, heightened cost and more material waste.


4. Admixture amount of curing agent and chemical reaction of silicon: e.g., mix100gof silicon with50gof silicon oil, after they are sufficiently and evenly mixed, add curing agent as per 2% of the total weight of silicon and silicon oil, mix again for 2-3 minutes before exhausting. Generally exhausting duration can not exceed 10 minutes; otherwise, the silicon will harden quickly to affect the quality of molding.



Need any help on silicone rubber, please feel free to contact Ms Lily:


Tel:86-755-89212369

Mob/Whatsapp:86-18938867593

E-mail: hyxe(at)szrl(dot)net

Skype:happynancy417



Send Inquiry

Product Alert

Subscribe to your interested keywords. We will send freely the latest and hottest products to your Inbox. Don't miss any trade information.

版权所有 © 宁波全贸信息技术有限公司 浙ICP备12012821号-1 浙B2-20200628