Specifications Ore Beneficiation / Hematite magnetic roasting / Iron Ore Beneficiation

Hematite magnetic roasting
 Overview     Hematite is weak magnetic associated ore. . The Mohs’ scale of hardness of the hematite is 6. The flow of the technics would be: 1st stage ore washing----storage----1st stage crushing----2nd stage crushing----3rd stage crushing----2nd stage ore washing----storage----feeding ore into rotary kiln----magnetizing roasting----ore cooling----storage----ore milling----magnetic separation----dehydrate----fine ore. The technics of coal powder making would be: coal storage----coal milling----coal powder concentrating----coal powder scaling----burning----tail gas processing.  Ore extracting and washing  Ore is transported to raw material storage by truck.The storage can be divided into three parts: raw ore storage, big size ore storage and washed ore storage. Ore is sent to raw material silo. At the top of the silo, it is a screen which can pick out ore with size bigger that 100mm. Ore bigger than 100mm will be sent to big size ore storage, while smaller than 100mm goes into the silo. There is a discharge opening at the bottom of the silo, through which the material can go into to a double screw sand washer to be washed. Given that the ore contains soil at a content of 60%, this sand washer is necessary to remove the soil and other impurity from the ore. The washed ore is sent to washed ore storage by belt conveyor. Washed ore with size bigger than 100mm will be sent to crushing silo. Under the opening of the silo is an vibrating feeder. We can adjust the vibrating amplitude of feeder to control the feeding speed. The feeder can separate the ore with size bigger or smaller than 40mm: the bigger one will be send to a crusher, smaller one to a circular vibrating screen. Ore Crushing and Storage Washed ore and ore bigger than 100mm are sent to a jaw crusher for first stage crushing. The output of first stage crushing is sent to second stage crushing, to be crushed into size smaller than 25mm. The output of second stage is sent to a  circular vibrating screen, which has two layers screen, 25mm and 10mm. Rock with size bigger than 25mm will be sent second stage for further crushing. Rock with size smaller than 25mm is sent to the 3rd stage crushing, hydraulic roller crusher, to be crushed into size no bigger than 10mm. Ore with size smaller than is sent to 2nd stage washing. The washed ore will be sent to a raw material silo, by belt conveyors buck elevators. We apply two flows in this plant; there should be a small silo at head of each rotary kiln. There are electromagnetic vibrating feeders at the bottom of silos to feed material into rotary kilns. Magnetizing Roasting and Cooling       Material, smaller than 10mm, is fed evenly to rotary kiln feeder by a valve feeder which is installed at the bottom of raw material silo. Then, the material is fed into  metallurgy rotary kiln. The ore reaction contains three stages: preheating, high-temp calcining, cooling. The temperature of high-temp calcining should be 900°C, and the time should be 30~60 minutes. After the reaction in the kiln, Fe2O3 become Fe3O4, which is magnetic. The reducers of this reaction would be C and CO. And the chemical reaction formula would be: 3Fe2O3+C→(600°)2Fe3O4+CO,3Fe2O3+CO→(600°)2Fe3O4+CO2 . While calcining, combined water of ore escapes, the grade of ore is improved. Magnetic ore goes through a discharge opening of rotary kiln into sand washer for cooling. This machine cools the magnetic ore to 100°C. After cooling, magnetic ore will be stored. The waste air come out of the rotary kiln will be purified and sent to the atmosphere. There is a tube connecting the end of rotary kiln and the coal mill, using the hot air in the kiln to dry the coal. Coal powder making and burning Coal requirement is: heat productivity no less than 6500Kcal/kg, size smaller than 10mm. Coal is elevated into the coal silo. There is a electromagnetic vibrating feeder, which feed the crushed coal into a coal mill, at the bottom of this silo. Coal is milled into powder in the coal mill. A blower press air to lift coal powder to a powder concentrator which picks out the qualified powder. The unqualified powder will be sent back for further milling by a screw conveyor. The qualified will be sent to a dust collector by air. The collected powder is stored in a silo. Under this silo, there is a coal powder scale system, which can adjust the coal powder feeding speed. Powder and air is sent to a burner buy a roots blower. The high temperature which this burner can generate is 1300°C. The tail gas of burning will go into a dust collector and the processed gas dust density is smaller than 200mg/m3 . Ore separation Magnetic ore is conveyed to a fine crusher first. The crushed magnetic ore is then stored in a silo. At the bottom of the silo, there is an electromagnetic feeder to control the feeding speed of magnetic ore. A belt conveyor transfer magnetic ore into wet type ball mill to be mill into 150 mesh. Then the slurry is send to a high type classifier. Qualified ore will run into a magnetic separator, unqualified will be sent back to ball mill for further milling. The magnetic separator’s magnetic density is 2400 Gauss. It can improve the Fe content in the ore up to about 50%, recovery rate about 90%. The tailing is sent and stored into a tailing pool. 50% Fe content ore slurry is then sent to the second stage magnetic separation, magnetic separator, 1800 Gauss. It can improve the Fe content up to about 60%, recovery rate about 93%. The final ore slurry is send to a disc type filter to dehydrate. The dry final ore contain moisture less than 5%. The tailings will be push to a disc type filter by a slurry pump for dehydration. The dried tailings can be stored for further usage. Ore Beneficiation / Hematite magnetic roasting / Iron Ore Beneficiation
Send Inquiry

Product Alert

Subscribe to your interested keywords. We will send freely the latest and hottest products to your Inbox. Don't miss any trade information.

版权所有 © 宁波全贸信息技术有限公司 浙ICP备12012821号-1 浙B2-20200628